Open Problems

Tractable Open

Where and when will a corrosion pit start?

Stainless steel and aluminium are protected by a thin oxide film that fails at isolated points, forming pits. How the film breaks down, and which sites become lasting pits, cannot yet be predicted.

corrosionmaterialselectrochemistry

On this page
  1. The problem
  2. Why it matters
  3. What counts as progress
  4. Known approaches
  5. Dead ends
  6. References
  7. Related problems
  8. Attempts (0)

The problem

Passive metals owe their corrosion resistance to an oxide film a few nanometres thick. In the presence of chloride and some other ions, the film breaks down locally and a small pit forms. Most pits stop growing and heal; a few become stable and can perforate a wall while the rest of the surface looks sound. Growth of an established pit is fairly well understood. The first step is not. Proposed mechanisms include ions passing through the film, thinning of the film by adsorbed ions, and repeated mechanical rupture. In real alloys pits usually start at inclusions and other defects, but which defects and why is only partly known. Engineers therefore treat pitting as a random process described by measured statistics.

Why it matters

Pitting causes leaks and can start cracks in pipelines, aircraft, chemical plant, medical implants and nuclear waste containers. Service life predictions over decades or longer need more than short laboratory statistics.

What counts as progress

  • Observations at the nanometre scale, in the corroding environment, of film breakdown at identified sites, linked to the local chemistry and structure before breakdown.
  • A model that predicts the distribution of pitting potentials or of times to first stable pit for an alloy from its measured inclusion population and the solution chemistry, tested on alloys not used to build it.
  • A clear experimental test that separates the proposed breakdown mechanisms for one well-defined system.
  • Open datasets of pit initiation events with full surface characterisation.

Known approaches

Electrochemical noise and potentiostatic transients; scanning probe and in-situ electron microscopy; point defect models of the film; atomistic simulation of chloride on oxide surfaces; statistical treatment of pit initiation and survival; high-throughput alloy screening.

Dead ends

A single pitting potential from one fast scan is not a material constant; it depends on scan rate, surface finish and specimen area. Ranking alloys by a composition index works within a family and fails across families and microstructures.

References

  1. Frankel (1998): Pitting Corrosion of Metals: A Review of the Critical Factors
  2. Wikipedia: Pitting corrosion